| Property | PP Homopolymer | PP + GF (30%) | |
| Mechanical Properties | Ultimate Tensile Strength | 30-35 MPa | 70-100 MPa |
| Yield Strength | 25-30 MPa | 60-80 MPa | |
| Hardness | 70-75 Rockwell R | 100-110 Rockwell R | |
| Elongation at Break | 200-600% | 2-3% | |
| Flexural Strength | 40-50 MPa | 120-150 MPa | |
| Modulus of Elasticity | 1.5-1.7 GPa | 4.0-5.0 GPa | |
| Wear Resistance | Fair | Good | |
| Machinability | Good | Good | |
| Physical Properties | Density | 0.90-0.91 g/cm³ | 1.10-1.15 g/cm³ |
| Impact Strength | Moderate | High | |
| Moisture Absorption | <0.02% | <0.02% | |
| Friction Coefficient | 0.30-0.40 | 0.25-0.30 | |
| Thermal Properties | Maximum Service Temperature | 100°C | 120°C |
| Thermal Expansion Coefficient | 100-150 x10⁻⁶/°C | 40-60 x10⁻⁶/°C | |
| Thermal Conductivity | 0.22 W/(m·°C) | 0.25 W/(m·°C) | |
| Electrical Properties | Dielectric Strength | Good | Good |
| Electrical Resistivity | 10¹⁶ Ω·cm | ~10¹⁵ Ω·cm | |
| Special Properties | UV Resistance | Poor (unless stabilized) | Moderate |
| Creep Resistance | Moderate | High | |
| Recyclability | Yes | Yes | |